Low Carbon Ferro Chrome 10-50mm Lumps

Low Carbon Ferro Chrome 10-50mm Lumps

The surface of ferrochrome must be cleaned of sand, slag and other foreign materials. Only oxide film and traces of non-stick materials are allowed. When breaking pieces, there should be no foreign inclusions.
जांच भेजें
विवरण
तकनीकी पैरामीटर
low carbon Ferro Chrome 10-50mm Lumps Description

 

 

Low Carbon Ferrochrome Pieces 10-50mm Manufacturers

Low Carbon Ferrochrome 10-50mm Manufacturers

 

 

 

The Specification Of low carbon Ferro Chrome 10-50mm Lumps

 

C

P

S

58-68

0.25-0.5

1.5-3.0

0.03-0.06

0.025-0.03

63-68

0.25-0.5

1.5-3.0

0.03-0.06

0.025-0.03

 

 

 

 

 

 